Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the wordpress-seo domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /var/www/html/wp-includes/functions.php on line 6260 Peel to Reveal Lip Masque - Happi
Skin Care

Peel to Reveal Lip Masque

Novel lip care formulation from Coast Southwest includes mango better and allantoin.

Released By Coast Southwest, Inc.

Peel to Reveal Lip Masque
Juta/Shutterstock.com
Ingredients
%

Phase A

  • Deionized Water (Water)
  • 69.90
  • Propylene Glycol USP (Propylene Glycol)
  • 6.00
  • Disodium EDTA
  • 0.10
  • 3V Allantoin (Coast Southwest, Inc., 3V Sigma USA) (Allantoin)
  • 0.05
  • Glycerin 99.7% USP (Coast Southwest, Inc.) (Glycerin)
  • 3.00

Phase B

  • Coast PVA-24 (Coast Southwest, Inc.) (Polyvinyl Alcohol)
  • 13.00

Phase C

  • Endicare TN (Coast Southwest, Inc.) (C12-15 Alkyl Benzoate)
  • 0.25
  • Endisil F-1000 (Coast Southwest, Inc.) (Dimethicone)
  • 1.00
  • Glossamer L6600 (Coast Southwest, Inc.) (Brassica Campestris/Aleurites Fordi Oil Copolymer)
  • 0.50
  • Cosmosil BS Oil - Babassu Oil (Coast Southwest, Inc., International Cosmetic Science Centre (ICSC)) (Orbignya Oleifera Seed Oil)
  • 2.00
  • Cosmosil MUR Oil - Murumuru Seed Oil (Coast Southwest, Inc., International Cosmetic Science Centre (ICSC)) (Astrocaryum Murumuru Seed Butter)
  • 1.00
  • Cosmosil 700 - Mango Butter (Coast Southwest, Inc., International Cosmetic Science Centre (ICSC)) (Mangifera Indica (Mango) Seed Butter)
  • 1.00
  • EndiMoist 3OS (Coast Southwest, Inc.) (Sodium Hyaluronate (and) Hydrolyzed Sodium Hyaluronate (and) Ricinus Communis (Castor) Seed Oil (and) Hydrogenated Castor Oil)
  • 1.00

Phase D

  • Flavor
  • 0.50

Phase E

  • Sharomix 704 (Coast Southwest, Sharon Personal Care) (Benzoic Acid (and) Sorbic Acid (and) Dehydroacetic Acid (and) Phenoxyethanol)
  • 0.70

Procedure

Phase A - Add Phase A with mixing to main vessel and mix at low speed and begin heating to 85-90ºC. Phase B - At 60-65ºC, begin adding Phase B to Phase A slowly allowing the polymer to dissolve. At 85ºC to 90ºC, hold the temperature and add any remaining Coast PVA-24 to the vessel and incorporate into the solution slowly. Once the addition is completed hold the temperature for at least 10 minutes then discontinue heat. Phase C - Cool to 70-75ºC. Add Phase C in formula order to Phase AB. The batch will turn opaque. Phase D - Cool the batch to 40-45ºC. Add Phase D followed by Phase E. Cool the batch to 25-30ºC, and transfer to a suitable vessel.

Properties

pH—5.5 to 6.0; Viscosity—spindle 6 @ 6.0 rpm = 70,000 to 100,000 cst.

Request more information from Coast Southwest, Inc.

Topics